http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021155618-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2ebdfc88803aa0e0bb776ddb9db35fda |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2020-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8c9a6494a6e84f18cf50ceb34d586d92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_14238a42ba7e40c61d81afb9f7886964 |
publicationDate | 2021-10-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2021155618-A |
titleOfInvention | Manufacturing method of propylene resin sheet |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a stretched propylene resin sheet having low orientation. A method for producing a propylene-based resin sheet, which comprises sequentially going through the following steps 1 to 3. Step 1: Obtaining a propylene-based resin film a containing smectic crystals using propylene-based resin A Step 2: Α crystals by heating the propylene-based resin film a at a temperature of 110 ° C. or higher and 140 ° C. or lower. Step 3: A step of obtaining a propylene-based resin film b containing [Selection diagram] Fig. 2 |