http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021138923-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b3ac2810a2592dd6d6ba33f68c226370 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C4-00 |
filingDate | 2021-01-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ec0ba53ab0a6d92582a280f1a884fc36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_713ca6a469cd7b021b5800873aecfff9 |
publicationDate | 2021-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2021138923-A |
titleOfInvention | Adhesive composition for unvulcanized rubber and its use |
abstract | PROBLEM TO BE SOLVED: To use an adhesive composition for unvulcanized rubber, which is excellent in adhesiveness and significantly reduces the problem of dust generation due to falling off, and an adhesive composition for unvulcanized rubber. Provided is a method for producing an unvulcanized rubber which has been subjected to an anti-adhesion treatment. SOLUTION: This is an adhesive composition for unsulfated rubber containing an inorganic component requiring a silicate and a surfactant, and the silicate contains at least one selected from iron oxide and iron sulfide. , The total weight ratio of the iron oxide and the iron sulfide to the total of the silicate, the iron oxide and the iron sulfide is less than 3% by weight, and the surfactants are anionic surfactants (A) and nonions. Adhesive composition for unsulfurized rubber containing the surfactant (B) and having a weight ratio (A / B) of 0.1 to 1 expressed by the weight of (A) / the weight of (B). .. [Selection diagram] None |
priorityDate | 2020-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |