http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021042350-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_527d41cad118be2c39e19a33eab54468 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M11-51 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B5-14 |
filingDate | 2020-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08accdd9d082c33688993567d4f62069 |
publicationDate | 2021-03-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2021042350-A |
titleOfInvention | Sulfate-esterified fibrous cellulose, composition, sheet and method for producing sulfate-esterified fibrous cellulose |
abstract | PROBLEM TO BE SOLVED: To suppress thermal decomposition of fine fibrous cellulose which has been sulfate-esterified. The present invention relates to a composition containing a carbamide group and having a fiber width of 1000 nm or less, a sulfate-esterified fibrous cellulose, a sulfate-esterified fibrous cellulose, and a sheet containing a sulfate-esterified fibrous cellulose. Further, the present invention is a step (a) of mixing a cellulose raw material with an aqueous solution containing sulfuric acid and / or sulfuric acid amide, and urea and / or a urea derivative, and heating the cellulose raw material at 100 ° C. or higher until the water content is substantially eliminated. It also relates to a method for producing sulfate-esterified fibrous cellulose, which comprises a step (b) of refining the cellulose raw material obtained in the step (a). [Selection diagram] None |