http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020536838-A

Outgoing Links

Predicate Object
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-24355
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K5-03
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C23-0075
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03B23-023
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B27-0006
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-18
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C19-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C03C15-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K7-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C15-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C17-32
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G06F3-041
filingDate 2017-12-21-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationDate 2020-12-17-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2020536838-A
titleOfInvention High-strength anti-fingerprint glass, its manufacturing method, high-strength anti-fingerprint glass exterior parts and its manufacturing method
abstract A high-strength anti-fingerprint glass comprising a glass substrate, the glass substrate comprising a first surface and a second surface provided oppositely, on at least one of the first surface and the second surface. microtexture structure is provided, microtexture structure includes a plurality of micro-texture units, orthogonal projection area of each micro-texture unit is in the range of 0.0004 mm 2 of 0.0144Mm 2, microtexture unit The range of maximum distances of the microtexture units associated with the placed surface is 2 μm to 7 μm. High-strength anti-fingerprint glass changes the physical structure of the glass surface due to the composition of the microtextured structure on the surface, thereby fundamentally solving the problem of fingerprints and oil stains that easily occur on the glass surface. Helps to significantly increase the impact resistance of glass.
priorityDate 2017-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017018692-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011530403-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013010684-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010254551-A
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015174428-A1
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010279068-A1
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID457280313
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID14917

Total number of triples: 27.