http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020510120-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2400-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F9-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F20-44 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F20-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-04 |
filingDate | 2018-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-04-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020510120-A |
titleOfInvention | Method for producing (meth) acrylonitrile-based polymer for producing carbon fiber |
abstract | The present invention includes a step of introducing a reaction solution containing a (meth) acrylonitrile-based monomer and a reaction solvent into a reactor to perform solution polymerization, wherein the viscosity of the reaction solution in the reactor is 0.1 poise to 250 poise. In some cases, solution polymerization is performed under the condition that the power consumption of the reactor is 1 to 5 kW / m 3 , and when the viscosity of the reaction solution in the reactor is more than 250 poise to 450 poise or less, the power consumption of the reactor is reduced. The present invention relates to a method for producing a (meth) acrylonitrile-based polymer for producing carbon fiber, wherein solution polymerization is carried out under the condition that is 8 to 13 kW / m 3 . |