abstract |
【Task】 A plastic alloy composition and a plastic alloy product are provided. [Solution] The plastic alloy composition of the present invention contains 60% of high-density polyethylene, 10% of polypropylene, 1% of triallyl isocyanurate, and 5% of polysulfone as components of the plastic alloy composition. , 10% ethylene-vinyl acetate and 14% color masterbatch. The ring stiffness of the siphon produced from the plastic alloy composition of the present invention is 7-8, the Shore hardness D is 77-80, the elongation at break is 100-500%, and the shrinkage is 0.5. % To 1%. The working temperature of the plastic alloy product of the present invention reaches 150 ° C. or higher, it has strong acid resistance and alkali resistance, and is excellent in impact resistance and pressure resistance. |