http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020204143-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H3-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H3-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D04H3-007 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H3-016 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H3-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H3-018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H3-033 |
filingDate | 2020-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_84dcddc378d1cc520c8c164f4f45d848 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_703b3af0810da4c18e0ae43e4ecc45dd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fd2127e6d5e0721ac1b1caba99bbdc75 |
publicationDate | 2020-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020204143-A |
titleOfInvention | Reticulated structure with excellent heat resistance and durability |
abstract | PROBLEM TO BE SOLVED: To provide a network structure using a polyolefin-based thermoplastic elastomer, which has a predetermined hardness and has a small compression residual strain even under high temperature and high humidity, and is suitable for applications such as cushions. Provided. SOLUTION: The network structure is obtained by cooling and then annealing a network structure having a three-dimensional random loop bonding structure composed of a polyolefin-based thermoplastic elastomer continuous linear body composed of an olefin block copolymer. The network structure has a fiber diameter of 0.1 to 3.0 mm, an apparent density of 0.005 to 0.20 g / cm 3 , a compressive residual strain at 70 ° C. of 30% or less, and a network structure. A network structure having an interfacial phase ratio of 40% or less obtained by measuring the resin constituting the body by a pulse NMR method. [Selection diagram] Fig. 1 |
priorityDate | 2014-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 55.