Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_669c01133740c5233f2c8738904ea3af |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G2-10 |
filingDate |
2020-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e3ca2add8a52547de45f0a869f75bde8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d29573cc98fa6f00be3eb7f9c2b56125 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f21dbf16932db95fd3917b7563334a37 |
publicationDate |
2020-12-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2020198305-A |
titleOfInvention |
Battery packaging material |
abstract |
PROBLEM TO BE SOLVED: To provide a packaging material for a battery which is less likely to cause pinholes and cracks during molding and has excellent moldability. SOLUTION: The base material layer 1 containing nylon, a metal layer 3 and a sealant layer 4 are sequentially laminated, and the base material layer is JIS Z1707: 1997 with respect to the thickness B of the base material layer. A battery packaging material having a piercing strength A ratio (A / B) of 0.92 N / μm or more, which is measured by a method according to the above. [Selection diagram] Fig. 1 |