http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020189416-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e77637bb8e9aefeb300ec46504f86589 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W90-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-102 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2019-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_687d90f86f8477a8b8328019bc2b6738 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ae45f49aad1b88772018446c17ad7133 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_712270921e0897ced52bb1e7a704dd7f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d2bcb5a8b9f2454581cd55fab57ba6a |
publicationDate | 2020-11-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020189416-A |
titleOfInvention | Laminates and packaging containers using them |
abstract | PROBLEM TO BE SOLVED: To provide a laminate having good adhesion to a barrier film and a packaging container using the same, an environment-friendly and highly safe laminate and a packaging container using the same. SOLUTION: The laminate has a film, a printing layer, an adhesive layer, and a base material in this order, and the printing layer has a colorant and a urethane group concentration of 0.3 to 2.4 mmol / g at the end. A polyurethane resin (A) having a urea bond having an amino group and a polyurethane resin (B) having a urethane group concentration of 3 to 6 mmol / g and not having a urea bond are contained, and the polyurethane resin (A) and polyurethane are contained. A laminate characterized by being formed of a printing ink composition for lamination containing a binder resin contained so that the mass ratio of the resin (B) is 95: 5 to 50:50. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023063090-A1 |
priorityDate | 2019-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 203.