http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020168837-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 |
filingDate | 2019-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9bf357fab7e5b0b99575eab32113ce20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02403f449d3f1c9e0d15e6a84ab8232a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0beb2a07bae2aa9643dc069be120b2de |
publicationDate | 2020-10-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020168837-A |
titleOfInvention | Gas barrier laminate, packaging material |
abstract | 【Task】 Provided are a laminate having excellent gas barrier properties and a small amount of solvent discharged during production, a method for producing the laminate, and a packaging material using the laminate. SOLUTION: A step of forming a printing layer on a base material using a water-based liquid ink, a step of applying a solvent-free gas barrier adhesive on a sealant layer to form a solvent-free gas barrier adhesive layer, and a solvent-free gas barrier property. A method for producing a laminate, which comprises a step of adhering a base material and a sealant layer via an adhesive layer. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022190999-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023181916-A1 |
priorityDate | 2019-04-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 282.