http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020158548-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J7-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B1-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-05 |
filingDate | 2019-03-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6c224b965e795ac9e0c6d64a246a0ebc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_051fce97d237e88f83f8856f0e405e2e |
publicationDate | 2020-10-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020158548-A |
titleOfInvention | Method of manufacturing a laminate |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a laminated body which is not hindered by curing from an adherend such as a polarizing plate even when the adhesive layer made of a photocurable silicone composition is cured at room temperature. SOLUTION: A method for producing a laminate comprising a base material and an adhesive layer laminated on the base material, wherein the adhesive layer is formed into a composition containing components (A) to (C) and has a peak wavelength of 380 to 420 nm. A manufacturing method of curing and forming by irradiating with the light of. (A) Polysiloxane (1) (R 1 R 2 2 SiO 1/2 ) a (R 2 3 SiO 1/2) 2-a (Ar 2 SiO 2/2) b (R 2 2 SiO 2/2) c (1) {R 1 is alkenyl, R 2 is alkyl, Ar is aryl, a is 0.3 to 2, b is 0 to 100, c is 1 to 1,000, and b / (b + c) = 0 to 0.7 is satisfied} (B) Hydrogen polysiloxane having at least two SiH bonds in one molecule (2) R 3 d H e SiO [( 4-de) / 2] (2) (R 3 is a monovalent hydrocarbon group excluding C = C group, d and e satisfy 0.7 ≤ d ≤ 2.5, 0.01 ≤ e ≤ 1.0, 0.8 ≤ d + e ≤ 2.7) (C) Platinum compound having at least one of β-diketonato, β-ketoesterate and 1,3-diesterate groups as a ligand [Selection diagram] None |