http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020139063-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b19eaa8e535da4e4bceed99917a68153 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-01 |
filingDate | 2019-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_80030c305dbcba249895d158029fec7c |
publicationDate | 2020-09-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020139063-A |
titleOfInvention | Resin composition and resin sheet |
abstract | PROBLEM TO BE SOLVED: To provide a resin composition and a resin sheet which can be laminated on a ceramic green sheet, have excellent followability to unevenness and smoothness of a surface, and suppress the occurrence of delamination at the time of cutting the laminated sheet. SOLUTION: A resin composition containing a resin component and a dielectric ceramic, having a thickness of 150 μm or more and 250 μm or less, a diameter of 18.5 mm, and a void ratio of 10% or less. While heating the plate-shaped resin composition to 80 ° C., the plate-shaped resin composition is sandwiched between metal plate-shaped pressing means whose facing surfaces are parallel to each other, and pressed at a pressure of 93.5 Mpa for 1 minute to obtain the obtained pressurization. When the object is viewed in a plan view from above, a resin composition having an area value of 4 cm 2 or more and 25 cm 2 or less of the pressurized object and a resin sheet using the resin composition are selected. [Selection diagram] None |
priorityDate | 2019-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |