http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020117729-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B7-027 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J183-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-38 |
filingDate | 2020-04-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a885bb18aa1ea70f338c1b9cc41a5d96 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_25606808337103b42bac1562d4645838 |
publicationDate | 2020-08-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020117729-A |
titleOfInvention | Silicone pressure-sensitive adhesive composition, pressure-sensitive adhesive article, laminate for optical device configuration, solar cell module, organic EL element, and method for producing laminate for optical device configuration |
abstract | PROBLEM TO BE SOLVED: To provide a pressure-sensitive adhesive article with a release film, which has both adhesive property at room temperature and low temperature property. SOLUTION: A linear organopolysiloxane (A) having a photoactive catalyst and (B) an organic functional group bonded to a silicon atom on a release film and curable by the photoactive catalyst, and (C) having an adhesive layer formed from a composition containing a branched organopolysiloxane, wherein the (B) linear organopolysiloxane and the (C) branched organopolysiloxane are incompatible The pressure-sensitive adhesive layer has a peak temperature of loss tangent at a frequency of 1 Hz measured by dynamic viscoelasticity after light irradiation under the following light irradiation conditions, from −140° C. to −100° C. or less, and −50° C. It is an adhesive article with a release film, which has one or more in the range of 100° C. or less and can be cured by light irradiation. [Light irradiation conditions] Ultraviolet rays are irradiated using a high-pressure mercury lamp so that the integrated light amount at a wavelength of 365 nm is 2 J/cm 2 . [Selection diagram] None |
priorityDate | 2015-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 67.