http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020109532-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-685 |
filingDate | 2020-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4ea90ff2781cdd04af2ea766c6f70f9b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_841006e0a39daf9f69e4a86a639d86fb |
publicationDate | 2020-07-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020109532-A |
titleOfInvention | Toner binder and toner |
abstract | PROBLEM TO BE SOLVED: To satisfy all of fluidity of toner, heat resistant storage stability, charge stability, pulverizability, image strength, bending resistance and document offsetting property while achieving both low temperature fixing property, glossiness and hot offset resistance. An object is to provide an excellent toner binder and toner. SOLUTION: The polyester resin (A) containing a carboxylic acid component (x), an alcohol component (y) and an oxazoline compound (a) as constituent raw materials is contained, and a differential scanning calorimetry is performed in a temperature range of -20°C to 80°C. It has at least one inflection point showing a glass transition temperature (Tg) on the chart by (DSC), the amide group concentration is 0.07 to 3.00 mmol/g, and the content of the surfactant is 100 ppm. A toner binder having the following characteristics is used. [Selection diagram] None |