http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020087846-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_440b3059c9bcd1d85fd383f9b2ae1b40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_bf9d28c1cfaed72a52604dd841454924 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-1069 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-1016 |
filingDate | 2018-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b5fa89289fbdb58c9b94d598b130e4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a5453620a2553577abfeb5848ffa1f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f90ec1c5195bd756ac994c6ff1417c32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8f7bbcf92336de74ecd4e12e45856e40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50e2c19b9f7071225bfd68f3e294b0a9 |
publicationDate | 2020-06-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020087846-A |
titleOfInvention | Method for manufacturing electrolyte layer |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing an electrolyte layer capable of forming a functional inorganic membrane on only one surface of an ion-exchange polymer membrane while suppressing damage to the ion-exchange polymer membrane. In manufacturing an electrolyte membrane (4) including an ion-exchangeable polymer membrane (16) and a functional inorganic membrane (17) arranged only on one surface thereof, the ion-exchangeable polymer membrane (16) and a frame-shaped jig (20). And the ion-exchangeable polymer film 16 is held by the frame-shaped jig 20, and the ion-exchangeable polymer film 16 is dipped and held in a metal ion solution of the element forming the functional inorganic film 17, The functional inorganic film 17 is formed on the surface of the exchangeable polymer film 16, and in the above dipping, the surface on one side of the ion exchangeable polymer film 16 and the metal ion solution are brought into contact with each other to form the ion exchangeable polymer film. An air pocket is formed on the other side of 16 to suppress contact between the other side surface of the ion exchange polymer membrane 16 and the metal ion solution. [Selection diagram] Fig. 3 |