abstract |
PROBLEM TO BE SOLVED: To effectively utilize clinker ash, which is an industrial waste that has not been used sufficiently so far, and to have sufficient strength without inhibiting the performance of open pores which is a characteristic of clinker ash. Further, since it can be molded and solidified by a simple operation, it provides a clinker ash molded body which consumes less energy and has a low manufacturing cost. SOLUTION: The main component is clinker ash, the bulk specific gravity is in the range of 1.2 to 1.6, the compressive strength is in the range of 1.8 to 12 MPa, and the apparent porosity is 32 to 46. It is characterized by being in the range of%. In addition, the water absorption rate is in the range of 20 to 35%. [Selection diagram] Figure 1 |