http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020056057-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e3b0a3dbf8d6c9712d86ea1383fd5327 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01R13-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D3-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01R43-16 |
filingDate | 2018-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_10d5e4dff91545f53df7a81d33226418 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_abf91c1c95c21bbc5b9997e081606fca |
publicationDate | 2020-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020056057-A |
titleOfInvention | Connector terminal material, connector terminal, and method of manufacturing connector terminal material |
abstract | An object of the present invention is to provide a connector terminal material capable of improving abrasion resistance and heat resistance, a connector terminal, and a method of manufacturing the connector terminal material. A terminal material for a connector according to the present invention includes a base material made of copper or a copper alloy, and a silver tin plating layer made of a silver tin alloy coated on at least a part of the surface of the base material, The silver-tin plating layer contains Ag in a range of 70 at% or more and 85 at% or less, contains silver-tin intermetallic compound as a main component, and heats the silver-tin plating layer at 150 ° C. for 250 hours. The average grain size of the crystal grains of the tin plating layer is 1 μm or less. [Selection diagram] Fig. 1 |
priorityDate | 2018-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |