http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020029511-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d2102ae92d209c2f12af9cc2e6c61b2f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 |
filingDate | 2018-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6bb768b55d1556eb8d4d4f2f2dd2b2ce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5f410c4835f3f56c797c1bb3932beb3f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_32caa108b94344d19cd0a9cd6411f461 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_385cc0992461d7d5540bb40f6eede778 |
publicationDate | 2020-02-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020029511-A |
titleOfInvention | Thermoplastic urethane resin |
abstract | An object of the present invention is to provide a thermoplastic urethane resin excellent in flexibility and low outgassing property and excellent in productivity of molded articles. A resin sheet having a thickness of 1.7 mm has a tensile modulus of elasticity (tension speed of 200 mm / min) of 3.3 MPa or less and a diffusion coefficient of less than 1.00 × 10 −11 m 2 / s. Is a thermoplastic urethane resin. The thermoplastic urethane resin preferably has a difference between a temperature [° C.] at which the storage elastic modulus E ′ is 1 MPa and a glass transition temperature [° C.] of 180 ° C. or more. The thermoplastic urethane resin preferably has a glass transition temperature of -10C or lower. [Selection diagram] None |