http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020026467-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6bfdf49224a405be1f7b653c56ebad94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L9-06 |
filingDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6dbfa25b4dcb538a49135a9e318d8107 |
publicationDate | 2020-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020026467-A |
titleOfInvention | Vulcanized rubber |
abstract | PROBLEM TO BE SOLVED: To provide a novel vulcanized rubber which is excellent in the modification of vibration damping property and excellent in balance of elongation, wear resistance and the like. SOLUTION: A peak of 5.8 to 6.5 ppm in a spectrum measured by 1 H-NMR in a partially hydrogenated dicyclopentadiene-based resin, preferably heavy chloroform at room temperature with respect to 100 parts by weight of rubber. The sum of the area (A) and the peak area (B) at 4.8 to 5.8 ppm is more than 0% and not more than 7.5% of the total peak area, and the peak area (A ) And 5 to 30 parts by weight of a partially hydrogenated dicyclopentadiene-based resin in which (A / B) expressed as a ratio of the peak area (B) is in the range of 0.01 to 0.2. . [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022255314-A1 |
priorityDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 42.