http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020025909-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D1-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-73 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B37-14 |
filingDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_607192ebbc1ee59bd35e4510ef2b9873 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5bf00e7cad38854c15f46585b00b3949 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cc39642499d4dd5999d313d74e064de1 |
publicationDate | 2020-02-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020025909-A |
titleOfInvention | Method for producing multilayer film and multilayer film |
abstract | An object of the present invention is to provide a method for producing a multilayer film having an intermediate coating layer having an appropriate pot life and excellent chemical resistance, and to provide the multilayer film. A method of manufacturing a multilayer film including an intermediate coating layer, a base layer laminated on the intermediate coating layer, and a clear layer laminated on the base layer. An intermediate coat is applied to the object 2 to form an intermediate coat 15, a base coat is applied on the intermediate coat 15, a base coat 16 is formed, and the base coat 15 is formed on the base coat 15. A clear paint is applied, a clear coat 17 is formed, and the intermediate coat 15, the base coat 16, and the clear coat 17 are cured by heating, and the intermediate coat has an intermediate base agent having a carboxyl group, An intermediate coating curing agent containing a carbodiimide-modified linear aliphatic diisocyanate, and a carboxyl group in the intermediate coating main agent, the molar ratio of the carbodiimide group in the intermediate coating curing agent is from 0.2 to 2.0. It is. [Selection diagram] Fig. 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022224306-A1 |
priorityDate | 2018-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 265.