http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020024872-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5c039f60302b61e712887aa2267ecbe
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-04
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-82
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-14
filingDate 2018-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ba2a68a17519efd4a8eb7d62f300cfa4
publicationDate 2020-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber JP-2020024872-A
titleOfInvention Power storage device
abstract A power storage device capable of preventing damage to an outermost layer electrode in a stacked body is provided. A power storage device (1) includes a laminate (2) formed by laminating a negative electrode (4), a positive electrode (5), a negative current collector (6), and a positive current collector (7), a laminate film (3) covering the laminate (2), and a negative current collector (11). 6 and a negative electrode tab 9 and a positive electrode tab 10 which are electrically connected to the positive electrode current collector 7 and are taken out of the laminate film 3. The laminate films 3 are opposed to each other in the stacking direction of the laminate 2. It has an upper exterior part 11 and a lower exterior part 12 arranged, and the upper exterior part 11 and the lower exterior part 12 have a substantially U-shaped cross section, and a laminating direction in the upper exterior part 11 and the lower exterior part 12. A dummy layer 23 is disposed between the inner wall surfaces 13a, 16a perpendicular to the upper surface and the upper end surface 2a and the lower end surface 2b of the laminate 2 in the laminating direction. , Negative electrode 4 and positive electrode viewed from the lamination direction Larger than the external dimensions. [Selection diagram] FIG.
priorityDate 2018-08-08-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID13652349
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID451953330
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID410553718
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID21881765

Total number of triples: 20.