http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020012215-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02J1-22 |
filingDate | 2018-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f27879b3f270c1f0790ae3862d0685fc |
publicationDate | 2020-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020012215-A |
titleOfInvention | Conductive para-type wholly aromatic polyamide multifilament and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a conductive para-type wholly aromatic polyamide multifilament fiber having a low electric resistance, a high fiber bundle strength and a large single-fiber fineness, and a method for stably producing the fiber for a long time. SOLUTION: The fiber is spun using a spinning solution prepared such that the content ratio of conductive particles in the fiber is 5% by weight or more and 20% by weight or less with respect to the polymer, and the single fiber fineness is 2.8 dtex or more by heating and drawing. A conductive para-type wholly aromatic polyamide multi-filament fiber having a fineness of 0 dtex or less and a total fineness of 60 dtex or more and 350 dtex or less is used. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022039033-A1 |
priorityDate | 2018-07-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 22.