http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020007493-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B15-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-04 |
filingDate | 2018-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6f452de079835f75b5afc801c6c4be5e |
publicationDate | 2020-01-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020007493-A |
titleOfInvention | Cellulose-containing resin composition |
abstract | An object of the present invention is to provide a resin composition having sufficient abrasion resistance in practical use and low odor while giving sufficient mechanical and thermal properties to the resin composition. (A) 100 parts by mass of a thermoplastic resin, (B) 1 to 200 parts by mass of cellulose nanofiber having an average fiber diameter of 1000 nm or less, and (C) 0.1 to 200 parts by mass of a surface modifier. And (D) 0.1 to 10000 ppm by mass of an organic solvent having a boiling point of less than 100 ° C. [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022215756-A1 |
priorityDate | 2018-07-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |