http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020002189-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f8877d26e7e712d48efb03a75bd073f3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 |
filingDate | 2018-06-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_64eb749320bc162634f988b444659573 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_52d1ab29b3946bb7b2378ee92842d056 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d689e1262044709af36540c3a2a76113 |
publicationDate | 2020-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020002189-A |
titleOfInvention | Method for producing polyglycolic acid resin composition |
abstract | An object of the present invention is to provide a method for producing a polyglycolic acid resin composition which has decomposability even in a low temperature environment and has excellent moldability. A method for producing a polyglycolic acid resin composition containing a polyglycolic acid resin and a decomposition accelerator for the polyglycolic acid resin, comprising: a first kneading step of melt-kneading the polyglycolic acid resin; A second kneading step of adding a decomposition accelerator to the kneaded polyglycolic acid resin and further melt-kneading, wherein the temperature of the kneaded material in the second kneading step is adjusted to 220 ° C or more and 270 ° C or less. . [Selection diagram] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114163791-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2022209885-A1 |