http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020001249-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M2-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-32 |
filingDate | 2018-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5afe8266e3a716414cacc7dbef2764c1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_214d019c857d0985e5607c7c5423a459 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_85a355fdef46c53d19090163c433341c |
publicationDate | 2020-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2020001249-A |
titleOfInvention | Porous film, separator for secondary battery and secondary battery |
abstract | An object of the present invention is to provide a porous film used for a separator for a secondary battery, which has high adhesiveness to an electrode and excellent battery characteristics. SOLUTION: A porous layer A is laminated on at least one side of a porous substrate, and (1) air permeability is 50 to 1000 sec / 100 cm 3 , (2) air permeability after heat treatment at 60 ° C. for 30 minutes. The air permeability is 1.05 times or more of the air permeability before the heat treatment. (3) After performing the heat treatment of the above (2), 25% is added to a solvent composed of at least one of dimethyl carbonate, ethyl methyl carbonate and diethyl carbonate. A porous film having an air permeability of 0.95 times or less before immersion at 24 ° C. for 24 hours. [Selection diagram] None |
priorityDate | 2018-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |