classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-145 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G9-145 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G9-035 |
filingDate | 2016-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-03-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019506743-A |
titleOfInvention | Electrolytic solution for aluminum electrolytic capacitor and aluminum electrolytic capacitor using the electrolytic solution |
abstract | The present invention relates to an electrolytic solution for an aluminum electrolytic capacitor containing a main solute and a main solvent, and further containing an additive represented by the following structural formula 1, and an aluminum electrolytic capacitor using the electrolytic solution. In the formula, R 1 and R 2 are each independently selected from —CH 3 , —CH 2 CH 3 or —OH, and R 3 and R 4 are each independently — (CH 2 CH 2 O) m H or —H. N and m are each an arbitrary integer of 1 to 10,000. The electrolytic solution of the present invention is excellent in corrosion resistance, can maintain a long load life when the chlorine ion content is high, and no trace of corrosion was observed in the dismantling capacitor. [Selection figure] None |
priorityDate | 2016-09-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |