http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019199550-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 |
filingDate | 2018-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0fd36aca19594aa88dffcba89c3a71a4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6d59df87ad63726c773307c3be068b0a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_efad6fb57627bdc601cd7e80f31eae72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_490fb9a878acab3c34382a11840c0450 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_587c3e63da6f626b6efea7f71a3fe9fa |
publicationDate | 2019-11-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019199550-A |
titleOfInvention | Method for producing olefin resin |
abstract | In the presence of a polymerization catalyst comprising a group 4 transition metal compound [A] containing a ligand having a dimethylsilylbisindenyl skeleton and a bridged metallocene compound [B] having a specific structure, In the reactor, ethylene and at least one α-olefin selected from α-olefins having 3 to 12 carbon atoms are copolymerized to produce an olefin resin satisfying the following requirements (I) to (IV): A method for producing an olefin resin. (I) Graft type olefin polymer [R1] comprised from a principal chain and a side chain is included. (II) The proportion of repeating units derived from ethylene is in the range of 50 to 90 mol% with respect to all repeating units, and the repeating is derived from at least one α-olefin selected from α-olefins having 3 to 12 carbon atoms. The ratio of the unit is in the range of 10 to 50 mol% with respect to all repeating units (however, the total of repeating units derived from ethylene and repeating units derived from α-olefins having 3 to 12 carbon atoms is 100 mol%). is there. (III) Melting | fusing point (Tm) measured by the differential scanning calorimetry (DSC) exists in the range of 0-100 degreeC. (IV) The intrinsic viscosity [η] measured in decalin at 135 ° C. is in the range of 0.1 to 10 dl / g. [Effect] According to the present invention, an olefin resin containing a graft type olefin polymer which is an ethylene / α-olefin copolymer having an amorphous side chain can be directly converted from a monomer into a single reactor in a single polymerization step. It can be manufactured and can be manufactured easily. [Selection figure] None |
priorityDate | 2018-05-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |