http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019188402-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6369b4272bab62999579e2fa142c6051 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-365 |
filingDate | 2018-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_08ccb5f2e6158e1c3d79f5970e9b7017 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_baf422315d4f9453ef012e4ad60cb6bf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c9d1225670b6f0eb114ec088aefc9b88 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8eba5bb73a700ea8605e67e0b72aa61 |
publicationDate | 2019-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019188402-A |
titleOfInvention | Coated arc welding rod for welding austenitic stainless steel |
abstract | PROBLEM TO BE SOLVED: To obtain a weld metal excellent in strength and toughness in both AC and DC welding power sources, excellent in weld defect resistance and hot crack resistance, and excellent in welding workability in all-position welding. A coated arc welding rod for welding is provided. SOLUTION: In one or both of a core wire and a coating agent, the core wire mass ratio is C: 0.04% or less, Si: 0.3-1.0%, Mn: 2-5%, Ni: 9- 12%, Cr: 18 to 24%, Al: 0.01 to 0.30%, Bi: 0.005 to 0.050%, and by weight based on the total mass of the coating, , TiO 2 converted value total: 20 to 40%, SiO 2 converted value total: 18 to 35%, Al 2 O 3 converted value total: 3 to 10%, F converted value total: 0.1 to 5 0.0%, CaCO 3 : 5 to 20%, a total of Na converted value and K converted value: 1 to 10%. [Selection figure] None |