http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019143071-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4e0fdb29eb5a277e1e02c130911173d3 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 |
filingDate | 2018-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e7726249013ef471f461288eff0da6a7 |
publicationDate | 2019-08-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019143071-A |
titleOfInvention | Adhesive resin composition, adhesive layer and laminate using the same |
abstract | An adhesive resin composition having high adhesion strength to a styrene resin layer and an ethylene / vinyl alcohol copolymer layer and excellent oil resistance without using a tackifier. A saturated polyester thermoplastic elastomer having a polyalkylene ether glycol segment content of 58 to 73% by mass is modified with an unsaturated carboxylic acid and / or a derivative thereof in the presence of a radical generator. The modified polyester elastomer (A) and the ethylene / vinyl acetate copolymer (B) having a vinyl acetate content of 15 to 50% by mass, the modified polyester elastomer (A) and the ethylene / vinyl acetate copolymer. The ratio of the modified polyester elastomer (A) in the total 100% by mass with (B) is 25 to 65% by mass, and the ratio of the ethylene / vinyl acetate copolymer (B) is 35 to 75% by mass. Composition. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023171792-A1 |
priorityDate | 2018-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 105.