http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019104933-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a2973a1bdaf87d5184fb1e81ebe5d061 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L65-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3492 |
filingDate | 2019-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e3f50f30a4a634a2da50a3dce4ea1db http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af5c57d2d894bcc0fc1cd451ccbc36c0 |
publicationDate | 2019-06-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019104933-A |
titleOfInvention | Polyacetal resin composition |
abstract | The object of the present invention is to provide a polyacetal resin which is excellent in mechanical properties and also excellent in hot water resistance. An object of the present invention is to use 1 part by mass or more and 100 parts by mass or less of glass fibers surface-treated with (B) a blocked isocyanate compound and an aminosilane coupling agent based on 100 parts by mass of (A) polyacetal resin And (C) boric acid 0.001 to 1.0 parts by mass, and the polyacetal resin (A) has a melt flow value of 35 g / 10 min at 190 ° C. under a load of 2160 g. This is achieved by the polyacetal resin composition being over 100 g / 10 min. 【Selection chart】 None |
priorityDate | 2019-04-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |