http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019099602-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 |
filingDate | 2017-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3c7f299a18f8178ef8a19b480a93444 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_967e414dd3f803329f79003996060432 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5c74628eb6ad34e43cc5fe309cd77986 |
publicationDate | 2019-06-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019099602-A |
titleOfInvention | Thermoplastic elastomer composition and molded article |
abstract | To provide a thermoplastic elastomer composition capable of obtaining a molded article excellent in heat aging resistance, gas barrier property, toughness, high temperature toughness and flexibility. SOLUTION: 10 to 50 parts by weight of a block copolymer (A) containing at least a polymer block mainly composed of an aromatic vinyl compound and a polymer block mainly composed of isobutylene, and 50 to 50 parts of a polyamide 610 resin (B) A thermoplastic elastomer composition comprising 20 to 100 parts by weight of a rubbery polymer (C) having a reactive functional group other than the block copolymer (A) with respect to a total of 100 parts by weight of 90 parts by weight. 【Selection chart】 None |
priorityDate | 2017-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |