http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019093443-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1837840b0d7f1d216335a0331a4bd15a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B23K35-363 |
filingDate | 2017-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_17e073c4375f13a6533bd5775f63788a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b772e7b2f10865b10f7c3c3c75e3436e |
publicationDate | 2019-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019093443-A |
titleOfInvention | Soldering flux |
abstract | An object of the present invention is to have high drying property in a heat treatment, good solderability, good wetting and spreading on a soldering surface, and no flash point, and uniform properties even when water is contained. Providing soldering flux with high electrical reliability. SOLUTION: An azeotropic mixture (A) containing a glycol compound (a1) having a boiling point of 120 to 200 ° C under normal pressure and water (a2) represented by the formula (1), and an activator (B) And the azeotropic point under normal pressure of the component (A) is 90 to 100 ° C. R 1 -O-[-CH 2 -CH 2 -O] n -R 2 (1) (n is 1 or 2; when n = 1, R 1 is H, R 2 is a C 1-4 alkyl group; When n = 2, R 1 is a C 1-3 alkyl group, R 2 is a C 1-3 alkyl group) 【Selection chart】 None |
priorityDate | 2017-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links