http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019090971-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8fb9f44db08d1c42a53f3d28eaae416f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-10 |
filingDate | 2017-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_73795c7cd96de84c6f3d15efa5094407 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2224584a4eca145c36eaa6312225be9e |
publicationDate | 2019-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019090971-A |
titleOfInvention | Liquid developer |
abstract | A liquid developer excellent in resin film adhesion of a fixed image and a printing method using the liquid developer. A liquid developer containing a toner particle containing a binder resin and a colorant, a dispersant, and an insulating liquid, wherein the binder resin is a polycondensation of a carboxylic acid component containing a polymerized fatty acid and an amine component. Liquid developer containing a polyamide resin having a storage elastic modulus of 2.0 × 10 8 Pa or less at 25 ° C., a toner particle containing a binder resin and a colorant, a dispersant, and a liquid containing an insulating liquid It is a developer, and when the binder resin is formed into a film and adhered to a film selected from a polyester film and a polypropylene film according to JIS K 6854-3: 1999, the maximum peel strength is 0.5 in conversion of 15 mm. A liquid developer having N or more and 10 N or less, and a printing method using the liquid developer. 【Selection chart】 None |
priorityDate | 2017-11-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |