http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019081963-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ef6afd894cd98832773642b0e1b5286e |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C25D11-16 |
filingDate | 2019-03-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e376b5203c945585c498773aeb2fab4c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f3b0cdbd39d3b55c8ef0abf52936644 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8c99bb3241ddefe71bce4773429b790 |
publicationDate | 2019-05-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019081963-A |
titleOfInvention | Alumite member, method of manufacturing alumite member and treating agent |
abstract | To provide an alumite member having excellent sealing property and corrosion resistance. SOLUTION: An alumite member has an anodic oxide film on the surface of an aluminum base or an aluminum alloy base, and is sealed with a component in which fluorine, cobalt and / or chromium are present, and does not contain nickel. The surface of the alumite member from the surface of the alumite member to the direction of the aluminum substrate or the aluminum alloy substrate, cobalt or chromium being present in the entire oxide film or in the thickness region of 0.01 μm or more; The content ratio of cobalt is 0.5% by mass or more and 40% by mass or less and / or the content ratio of chromium is 1% by mass or more and 40% by mass or less. [Selected figure] Figure 2 |