http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019079747-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7af673589ca45d2fd8b9ea902cdbd1dc |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-12 |
filingDate | 2017-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a90f62fd2344a21d039affbdd22cff8 |
publicationDate | 2019-05-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019079747-A |
titleOfInvention | CATHODE FOR SOLID OXIDE FUEL CELL AND SOLID OXIDE FUEL CELL SINGLE CELL |
abstract | PROBLEM TO BE SOLVED: To provide a cathode for a solid oxide fuel cell which can simultaneously suppress the separation of the cathode and the reduction of the power generation performance due to the introduction of a crack in the cathode, and a solid oxide fuel cell single cell using the same. Do. A cathode 1 is formed on a film surface of a cathode body 10 in the form of a film to which an oxidizing gas A is supplied from the outside, and the cathode body 10, and is for contacting a current collector 6. And a plurality of current collector contact portions 11. The cathode body 10 has a plurality of domain regions 102 surrounded by the cracks 101 introduced in the film thickness direction, and the cathode 1 has a 50% cumulative average diameter D of the domain regions 102, a current collector contact When the average distance between the parts 11 is L, the relationship of L ≦ D is satisfied. The unit cell 5 has a cathode 1. [Selected figure] Figure 1 |