Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d5c039f60302b61e712887aa2267ecbe |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P70-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-52 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-30 |
filingDate |
2017-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3b89758af96f5182b5e21d6750a3b8b3 |
publicationDate |
2019-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2019071238-A |
titleOfInvention |
Method of manufacturing nickel metal hydride battery |
abstract |
A low resistance nickel metal hydride battery is provided. [Solution means] a) assembling a nickel metal hydride battery containing cobalt at the positive electrode, b) a) a charging step of charging the nickel metal hydride battery after the step, the charging step including a voltage holding step of holding a voltage within a range of 0.8 V to 1.2 V for 1 to 100 hours; A method of manufacturing a nickel metal hydride battery, comprising: [Selected figure] Figure 1 |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7223721-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2021174743-A |
priorityDate |
2017-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |