http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019070086-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f1dd1d9a6cdaa14f3cd103c75d09d35 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F11-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-40 |
filingDate | 2017-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ab424ab78611cdcbfc3c1f8d814e6f64 |
publicationDate | 2019-05-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019070086-A |
titleOfInvention | Method of producing extender pigment, and extender pigment |
abstract | An object of the present invention is to uniformly disperse a crushed product of dolomite, which is an extender pigment, in a medium. [Solution means] The white dolomite is ground to 1 to 50 μm and the ground 1 is wetted with water. Then, the dispersing agent 3 is sprayed from above while being put in a heated stirrer 4 and stirred, and made into a paste. Then, when the paste-like pulverized material 1 reaches 60 ° C., the stirring is stopped, and then the pulverized material 1 with the dispersing agent 3 attached to the surface is dried, put into the solvent of the paint, Stir with dispersant, stabilizers, etc. [Selected figure] Figure 1 |