http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019055904-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8527eff5e19b189ce5818275e93dd90e http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0950e9df7f0e1b73efee1bda859951ad |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P40-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B28B3-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-26 |
filingDate | 2017-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4f13a6dcc15c500f1070e4e3e455eaae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4904d1df451a36b118e1364fb213265d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_09522d4d3d5147e12fbfaf43e157fb0b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_21bed769d398e39951f2685835155f93 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c26c6f58d7450247f3303f6240e1fb0a |
publicationDate | 2019-04-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019055904-A |
titleOfInvention | Geopolymer molded body manufacturing method and geopolymer molded body manufacturing system |
abstract | [PROBLEMS] To provide a geopolymer molded product having a long mixing time of a solidifying material and an alkali stimulant, requiring less energy for producing a solidified product, and having a short time required for producing a solidified product. Providing manufacturing methods and the like. A method of manufacturing a geopolymer molded body according to an embodiment includes a mixing step and a compression step. In the mixing step, a mixture is obtained by mixing the solidifying material and the alkali stimulant. In the compression step, a geopolymer molded body is formed by compressing and molding the mixture. Here, the alkaline stimulant includes a hydrate. And when compression of a mixture is performed in a compression process, a mixture is heated so that crystal water may detach | desorb from a hydrate, and reaction between a solidification material and the said alkali stimulant advances. [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-112020001453-T5 |
priorityDate | 2017-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.