http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019014818-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95585944cd76ddfb6dc33ed2a0b84403 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-205 |
filingDate | 2017-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b4b92dbf068dcd139c6bacfc632dd34f |
publicationDate | 2019-01-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2019014818-A |
titleOfInvention | Solid polypropylene resin composition |
abstract | Provided is a solid resin composition (preferably a masterbatch pellet) having excellent handling properties containing an additive which is liquid at room temperature. Melting obtained from a melting endotherm curve obtained by using a differential scanning calorimeter (DSC) and holding the sample at −10 ° C. for 5 minutes in a nitrogen atmosphere and then raising the temperature at 10 ° C./min. 10% by mass or more and 99.6% by mass or less of a polypropylene resin (A) having an endothermic amount (ΔH-D) of 0 J / g or more and 80 J / g or less, and an additive (B) that is liquid at 23 ° C. A solid polypropylene resin composition containing 4% by mass or more and 90% by mass or less. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102129411-B1 |
priorityDate | 2017-07-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 296.