http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018514602-A
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2170-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J2301-302 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-672 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-067 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D175-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F290-067 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4236 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J175-16 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F290-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-04 |
filingDate | 2016-03-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018514602-A |
titleOfInvention | Pressure sensitive adhesive |
abstract | At least one urethane (meth) acrylate oligomer having a molecular weight between about 2,000 g / mol and about 50,000 g / mol and an OH number of 0.01 mg KOH / g to 100 mg KOH / g, at least one mono (meta) ) A pressure sensitive adhesive (PSA) composition comprising an acrylate functional monomer and at least one tackifying resin. The PSA system may optionally also contain other additives such as at least one initiator system comprising at least one photoinitiator or free radical initiator. The PSA system is liquid at a temperature of 25 ° C. ± 2 ° C., has a viscosity of 15,000 cPs or less, and is adapted to form a smooth and uniform coating or film when cured without the application of heat. The resulting film has advantageous properties with respect to peel strength, tackiness and shear resistance. In embodiments, the PSA system contains less than 1 wt% solvent and less than 1 wt% water, or no solvent and no water. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102020182-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113929812-A |
priorityDate | 2015-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 83.