http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018203875-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C10G1-00 |
filingDate | 2017-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53ba801011f25c68c1c00e810321ce2e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_48c180256da875d3372590050706aeaf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2dbddf75c25689b49c0e87c25457ef2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f7b9c8260b20afb2e634b8fd1de58e92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4418b8d764c8154c25c12d363010fbec |
publicationDate | 2018-12-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018203875-A |
titleOfInvention | Method for producing bio-oil using metal and method for modifying bio-oil |
abstract | 【Task】 The present invention provides a method for producing biooil in a high yield by pyrolyzing biomass, and a method for producing olefin and / or aromatic hydrocarbon from the biooil efficiently. [Solution] Biomass in the presence of water and / or water vapor, iron and at least one metal selected from Group 5 to 11 of the long-period periodic table, the molar ratio (metal / iron) is 0.001 to 0 A method for producing bio-oil, characterized by adding in the range of .9. [Selection figure] None |