http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018197339-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10761 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L29-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B32B17-10605 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C03C27-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2018-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81deb314371f9777c1edc6f702fc3ea8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a2e97b387449e7de817ee0bfc0f11097 |
publicationDate | 2018-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018197339-A |
titleOfInvention | Sheet manufacturing method, recycling method and sheet |
abstract | An object of the present invention is to obtain a sheet having excellent transparency using a polyvinyl acetal resin generated in the process of producing an interlayer film for laminated glass. The method includes melt-kneading and extruding a polyvinyl acetal resin composition containing a polyvinyl acetal resin having a different average residual hydroxyl group amount and a plasticizer, which is generated in the process of producing an interlayer film for laminated glass. The present invention relates to a sheet manufacturing method. The resin composition has an average residual hydroxyl group amount Y mol% (Y is a positive number) with respect to 100 parts by mass of polyvinyl acetal (A) having an average residual hydroxyl group amount X mol% (X is a positive number). And it is preferable that 3-100 mass parts of polyvinyl acetals (B) which satisfy | fill | X-Y |> = 3 are included. [Selection figure] None |