http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018197308-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4c78a658c1bead8649e1fb51a9d492f7 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J167-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 |
filingDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f54069ae96d8e42bd83e52fbb02d7cb5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c8d5d546bc9cdfd065f76c4a86490af8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_91f5fc4735bac4f0ef6019f3d1126e0f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_509d769f1adadc2212a2435724d2d6a2 |
publicationDate | 2018-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018197308-A |
titleOfInvention | Two-component laminating adhesive composition and laminating film |
abstract | The object of the present invention is to achieve a low laminating temperature while combining strong adhesion between a metal plate / resin film, laminating suitability, blocking property, processing part boiling property and excellent productivity, An object of the present invention is to provide a two-component curable laminate adhesive composition capable of expressing a high-quality design of a resin film. A polyester resin having a specific molecular weight and a glass transition temperature (Tg), two types of blocked isocyanates having a dissociation temperature range of 100 to 120 ° C. and a dissociation temperature range of 140 to 160 ° C., an amine catalyst (D ), Containing a polyisocyanate compound (E), and the degree of softening of the film under the condition of 100 ° C. to 240 ° C. is 80% or more, and after heating at 100 ° C. to 240 ° C. for 30 seconds to 120 seconds, A two-component laminating adhesive composition having a film softening degree of 40% or less under conditions, and further having a gel fraction of 70% or more after being held at 40 ° C. for 5 days or heated at 230 ° C. for 30 seconds. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2021200714-A1 |
priorityDate | 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 188.