http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018178120-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6941b41269178b23247cc580fc19bb94 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-17 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L33-00 |
filingDate | 2018-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fedc84734a40b2e3d841ec79f056bb4 |
publicationDate | 2018-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018178120-A |
titleOfInvention | Curable composition and joint structure using the same |
abstract | PROBLEM TO BE SOLVED: To provide a curable composition which is cured by moisture in the atmosphere to give a cured product having an excellent antifouling effect. SOLUTION: The curable composition of the present invention comprises a polymer having a hydrolyzable silyl group containing a polyalkylene oxide (A) having a hydrolyzable silyl group, and a sucrose fatty acid ester type surfactant (C). And the cured product of the curable composition is excellent in the antifouling effect, and adhesion of dust and contaminants to the cured product is suppressed, and a beautiful appearance is maintained over a long period of time. Do. [Selected figure] None |
priorityDate | 2017-04-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |