http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018177912-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_efbfdc7316d3b1b7ceaee5366a61b6e0 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02T10-86 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08C19-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B60C1-00 |
filingDate | 2017-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_324b91057f3fa80b66de35c9c2479e68 |
publicationDate | 2018-11-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018177912-A |
titleOfInvention | Method for producing modified diene polymer, modified diene polymer, rubber composition and tire |
abstract | An object of the present invention is to provide a method for producing a modified diene-based polymer capable of obtaining a modified diene-based polymer which can be made into a rubber composition excellent in low and low loss properties when used together with a reinforcing filler. Provided. A process for producing a diene polymer containing 1,3-butadiene, and 3,6-di (2-pyridyl) -1,2 with respect to 100 parts by mass of the produced diene polymer. 0.01 to 2.5 parts by mass of a tetrazine compound which is at least one selected from 4,4,5-tetrazine and 3,6-di (4-pyridyl) -1,2,4,5-tetrazine And heating the mixture to modify the diene polymer. A method of producing a modified diene-based copolymer, wherein the diene-based polymer further contains an aromatic vinyl compound, preferably styrene. 【Selection chart】 None |
priorityDate | 2017-04-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 615.