http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018172809-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M15-227 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-06 |
filingDate | 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8dfb75305eedf216a3c607d63004544d |
publicationDate | 2018-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018172809-A |
titleOfInvention | Reinforcing fiber bundle, molding material and molded body |
abstract | An object of the present invention is to provide a reinforcing fiber bundle having excellent adhesiveness with a thermoplastic resin and good handleability. The structural unit derived from butene of an olefin component is more than 50 mol% and 100 mol% or less, and the melt flow rate (MFR) determined under conditions of 190 ° C. and 2.16 kg load according to the ASTM 1238 standard. ) To 100 parts by mass of butene-based resin (A) in the range of 0.01 to 20 g / 10 minutes, and a mixture containing at least 3 to 50 parts by mass of olefin-based resin (B) is adhered as an adhering substance. A reinforced fiber bundle, wherein the MFR of the butene resin (A) is smaller than the MFR of the olefin resin (B), and the olefin resin (B) contains at least a carboxylate bonded to the polymer chain. It is a reinforced fiber bundle that is a resin, and the amount of deposit that is a mixture of butene-based resin (A) and olefin-based resin (B) is in the range of 0.3 to 5% by mass. . [Selection figure] None |
priorityDate | 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |