http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018172177-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e2b60c751b9b6855cd19a5127595779f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 |
filingDate | 2018-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d4d6c4d3cde8e2fda40410fddd1ed736 |
publicationDate | 2018-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018172177-A |
titleOfInvention | Polyethylene for high-purity chemical containers and high-purity chemical containers |
abstract | Polyethylene for high-purity chemical containers having excellent moldability and environmental stress cracking resistance (ESCR), with less content of metal-derived components derived from polyethylene resin and polymerization catalyst components in stored and stored contents, and Provide high-purity chemical containers. An ethylene polymer (A) having a density (d) of 0.930 to 0.950 g / cm 3 , an HLMFR of 0.1 to 1 g / 10 minutes, and a density (d) of 25 to 49% by mass. 51-75% by mass of an ethylene polymer (B) having a melt flow rate (MFR) of 1-50 g / 10 min measured at 0.960-0.970 g / cm 3 , a temperature of 190 ° C., and a load of 2.16 kg. Provided by polyethylene which is included as an essential component and satisfies specific requirements at the same time. [Selection figure] None |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7243223-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020116912-A |
priorityDate | 2017-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |