http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018171724-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_b19eaa8e535da4e4bceed99917a68153 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B11-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H13-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D04H1-4209 |
filingDate | 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3aa7b1bcff6b839afff7210e287c22ba |
publicationDate | 2018-11-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018171724-A |
titleOfInvention | Method for producing composite |
abstract | Disclosed is a method for producing a composite, which can suppress uneven distribution of fibers and resins of a composite including fibers and a resin and reduce variations in mechanical properties of a molded product obtained from the composite. A method of manufacturing a composite of the present invention is a method of manufacturing a composite including a resin and a fiber, the step of adding a resin and a fiber to a solvent and stirring to obtain a slurry, through a filter The separation rate in the step of separating the solvent from the slurry and the step of obtaining the agglomerate and the step of drying the agglomerate, and separating the solvent from the slurry is 3 cm / min or more and 60 cm / min or less. [Selection] Figure 2 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2023100820-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113942139-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113942139-A |
priorityDate | 2017-03-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 60.