assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G06F3-041 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C14-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B15-082 |
filingDate | 2017-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dc02ea7343a2af6594e569a7d0b0558e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c537462d75d797f2855d1436f83e6fe http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_306dcff8ba77eaad24588537afe76be7 |
publicationDate | 2018-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018167423-A |
titleOfInvention | Conductive laminate |
abstract | To obtain a conductive laminate having an ITO film in which crystallinity is further lowered as compared with an ITO film obtained by normal addition of water. A conductive laminate having a transparent conductive layer made of tin oxide-added indium oxide having substantially the same composition on at least one surface of a resin base material, the transparent conductive layer being arranged in a thickness direction. The hydrogen atom concentration changes, has a maximum hydrogen atom concentration at the center in the thickness direction, and the difference between the maximum value and minimum value of the hydrogen atom concentration is 1.0 × 10 17 atoms / cc or more. Laminate. [Selection figure] None |
priorityDate | 2017-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |