http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2018165017-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_27aa3092499b93e3144b5053272698ca |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 |
filingDate | 2017-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_549cdf1a14c2648890f15348e47f0060 |
publicationDate | 2018-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2018165017-A |
titleOfInvention | Method for producing film laminate |
abstract | Film lamination excellent in interlayer adhesion by insert molding of a polycarbonate resin composition (A) containing a styrene resin having a copolymer component of a bisphenol C type polycarbonate resin and an α, β-unsaturated dicarboxylic acid component Manufacture the body. [MEANS FOR SOLVING PROBLEMS] A film (B) made of bilphenol A-type polycarbonate resin is loaded into dies 1A and 1B, and an injection molding temperature of the polycarbonate resin composition (A) is (280 ± a) ° C. And the surface temperature of the film (B) is (120−a / 2) ° C. or higher and the glass transition temperature (Tg) or lower of the polycarbonate resin composition (B). [Selection] Figure 1 |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020138451-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7135937-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7135972-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2020163597-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-7249593-B2 |
priorityDate | 2017-03-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 212.